PENGARUH VARIASI KADAR SUPERPLASTICIZER TERHADAP KUAT TEKAN BETON DENGAN CAMPURAN SILICAFUME 10% AGREGAT MAKSIMUM 20 MM (DENGAN METODE ERNTROY & SHACKLOCK)
PENELITIAN INI BERTUJUAN UNTUK MENGETAHUI PENGARUH VARIASI KADAR SUPERPLASTICIZER TERHADAP KUAT TEKAN BETON DENGAN CAMPURAN SILICAFUME 10% AGREGAT MAKSIMUM 20 MM (DENGAN METODE ERNTROY & SHACKLOCK)
Main Author: | FAISAL RIZA |
---|---|
Format: | SKRIPSI PRA 2008 |
Language: | Bahasa Indonesia |
Published: |
Universitas Muhammadiyah Yogyakarta
2008
|
Online Access: |
http://oaipmh-jogjalib.umy.ac.idkatalog.php?opo=lihatDetilKatalog&id=69056 |
Similar Items
-
PENGARUH VARIASI KADAR SUPERPLASTICIZER TERHADAP KUAT TEKAN BETON DENGAN CAMPURAN SILICAFUME 10% AGREGAT MAKSIMUM 20 MM (DENGAN METODE ERNTROY & SHACKLOCK)
by: FAISAL RIZA
Published: (2008) -
PENGARUH VARIASI KADAR SILICAFUME TERHADAP KUAT TEKAN BETON DENGAN CAMPURAN SUPERPLASTICIZER 2% AGREGAT MAKSIMUM 10 MM (Dengan Metode Erntroy dan Shacklock )
by: Andry Wiryanto
Published: (2008) -
PENGARUH VARIASI KADAR SILICAFUME TERHADAP KUAT TEKAN BETON DENGAN CAMPURAN SUPERPLASTICIZER 2% AGREGAT MAKSIMUM 10 MM (Dengan Metode Erntroy dan Shacklock )
by: Andry Wiryanto
Published: (2008) -
PENGARUH VARIASI UMUR BETON TERHADAP KUAT TEKAN BETON ( fc' ) DENGAN CAMPURAN SILICAFUME 10% DAN SUPERPLATICIZER 2% GRADASI AGREGAT MAKSIMUM 10 MM
( Dengan Metode Erntroy dan Shacklock )
by: Wawan Kurniawan
Published: (2008) -
PENGARUH VARIASI UMUR BETON TERHADAP KUAT TEKAN BETON ( fc' ) DENGAN CAMPURAN SILICAFUME 10% DAN SUPERPLATICIZER 2% GRADASI AGREGAT MAKSIMUM 10 MM
( Dengan Metode Erntroy dan Shacklock )
by: Wawan Kurniawan
Published: (2008)